Damage
2 cases · 5 images for “embrittlement”
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Damage — sub-branches

ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking

ML00088 / Dec.2017
Hydrogen Cracking of an API 5D S135 Drill Pipe
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
More from these cases

ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking

ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Transgranular Cracking

ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Transgranular Crack