Damage
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure: Segregation Bands ×Standard: Modified ×Capture method: Aspect Before Analysis ×clear all
Damage — sub-branches

ML00159 / Mar.2020
Collapse of a Drill Pipe
M - Low Alloy Medium Carbon QTP - Drill PipeAp - O&G Well DrillingCd - Ductile Behavior
Cm - Aspect Before AnalysisDf - General View
More from these cases

ML00159 / Mar.2020
Collapse of a Drill Pipe
M - Low Alloy Medium Carbon QTP - Drill PipeAp - O&G Well DrillingCd - Ductile Behavior
Cm - Aspect Before AnalysisDf - Fracture