Damage

1 case · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Ductile Fracture

More from these cases

ML00143 — Impact of a .308 Winchester on A36 PlateM - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples