Damage

2 cases · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Gas piping.  Aspect of a branching line 2" ND, lateral to a horizontal main pipe ND 8", welded using a weldolet. The cracking started at the margin of the weld in the upper part of the pipe, where the weld crossed the longitudinal direction of the pipe, perpendicular to the branch.
932
ML00149 / Dec.2018
Vibration Induced Fatigue in a Gas Piping
M - Low Carbon SteelP - Piping spoolAp - FPSOCd - Vibration Induced Fatigue
Cm - Aspect Before AnalysisDf - Cracking
Aspect of the heat exchanger plate showing the rupture of the plate in multiple cracks, starting at the side of the crude oil with high salinity.
727
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking