Corrosion

3 cases · 12 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
Micrography of the flange in the longitudinal section. The flange microstructure is ferritic austenitic, presenting a coarse structure.
102
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure

More from these cases

ML00095 — MIC of a Riser Control LineM - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Fusion Line
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Fusion Line
ML00094 — MIC of a Subsea Hydraulic LineM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Grain refined structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Strain Hardened
ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Micrographic detail of the flange microstructure in the longitudinal section. The flange is ferritic austenitic, presenting 70% of austenite. In the ferrite network there are evidences of precipitation/formation of detrimental phases.
113
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
Micrographic detail of the flange microstructure in the longitudinal section. The flange is ferritic austenitic, presenting 70% of austenite. In the ferrite network there are evidences of precipitation/formation of detrimental phases.
100
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Electrolytic Etch Micrography by SEMDf - Delta ferrite