Corrosion

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks

More from these cases

ML00085 — Corrosion Fatigue of a Martensitic SS PinM - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks