Stress Corrosion

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Schematic drawing presenting the longitudinal section of the shell plate (sample removed from the boiler), at the position of the fillet weld (sealing weld) with a tube,  where surface welding repairs created conditions for cracking the base material in a transgranular morphology. Several cracks were identify starting from the steam drum internal surface.
120
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Identification drawingDf - Cracks