ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M
- Austenitic Stainless Steel
P
- Bolt
Ap
- Oil and Gas
Cd
- Stress Corrosion
Cm
- Surface Aspect
Df
- Low Mag