Crevice Corrosion in a Subsea System — Aspect Before Analysis

Scanning Electron Microscope — sub-branches

ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
The scanning electron microscopy image of the internal surface of the tube in position 2 shows a localized  corrosion region with intergranular morphology, as well a crack from the corroded region.
1237
ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Surface Aspect by SEMDf - Intergranular Corrosion

More from these cases

ML00086 — Intergranular Corrosion of Sensitized 304SSM - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
The low magnification image of the internal surface of the tube, in position 2, shows several points of localized corrosion, with intergranular morphology.
193
ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Surface Aspect by SEMDf - Intergranular Corrosion