Crevice Corrosion in a Subsea System — Aspect Before Analysis

The micrography in the as polished condition of the longitudinal section of the pipe close to the washout, shows that at the tool mark tip (notch from the external surface) a fatigue crack already started from a corroded region (pitting).
187
ML00068 / Sep.2020
Corrosion Fatigue of a 5" Drill Pipe
M - Low Alloy Medium Carbon QTP - Seamless PipeAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Micrography by OMDf - Pitting
Micrographic aspect of the corrosion damage in a section transverse to the pitting.
167
ML00054 / Dec.2018
Cutlery Corrosion
M - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Pitting