Optical Microscope

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Optical Microscope — sub-branches

The micrography of the longitudinal section of the tube, close to OD, shows the paralel cracks, filled with oxides, perpendicular to the surface.
1444
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Close to the External Surface