Optical Microscope

3 cases · 3 images for “embrittlement”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Brittle Cracks
Multiple intergranular cracks transverse to the bolt axis. Hydrogen assisted cracking due to cathodic protection of a high strenght steel. Micrography in the "as polished" condition.
104
ML00077 / Jun.2018
Hydrogen Cracking of LAS Subsea Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Micrography by OMDf - Brittle Cracks
ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Brittle Cracks