Optical Microscope

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Optical Microscope — sub-branches

Micrography of the weld metal presenting a martensitic island with microcracks, due to a localized increase in the manganese and silicon content, probably because an active flux was adopted in a condition where a high cleanning action was not required. A high flux-to-wire ratio (>1) could also be an issue.
794
ML00067 / May.2017
Cold Cracks in C-Mn SAW Weld Metal
M - CMn SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Microcracks