Optical Microscope
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Welding Defect ×Microstructure: Ferritic ×Detail focus: Intergranular Cracking ×clear all
Optical Microscope — sub-branches

ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Intergranular Cracking
More from these cases

ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Intergranular Cracking