Optical Microscope
3 cases · 30 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Optical Microscope — sub-branches

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - At the Surface

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
More from these cases

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - Martensite

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - Bainitic Martensitic

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - Secondary Cracks
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - Bainitic Martensitic

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Pearlite

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Strain Hardened

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - At the Surface

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Oxide Layer

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Non Hardened Surface

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation