Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of the elbow base metal. The comparison with the pipe micrography shows an important difference of thickness.
132
ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Base Metal Right Side
Micrography of a longitudinal section of the pipe AA 6063. Granular structure and dispersed particles.
169
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Base Metal Right Side

More from these cases

ML00065 — Erosion Corrosion of Monel PipingM - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Elbow base metal micrographic detail presenting a granular microstructure. Like the pipe, the microstructure reveals inclusions.
106
ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion