Oxalic Acid Electrolytic Etch
6 cases · 10 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
More from these cases

ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite