Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Fusion Line
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line

More from these cases

ML00053 — SAW Longitudinal Seam of X70 PipeM - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line