Micrography by OM using A262 Method A
2 cases · 3 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Branched Cracks

ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Branched Cracks
More from these cases

ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Branched Cracks