Kalling Etched Micrography by OM
1 case · 6 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Banded Structure
More from these cases

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Banded Structure

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Banded Structure

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Banded Structure

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect