ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M
- Aluminum Bronze
P
- Seamless tube
Ap
- Oil and Gas
Cd
- Stress Corrosion
Cm
- As polished micrography
Df
- Cracking