Longitudinal Section Aspect
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Capture method
/
Naked Eye or Stereoscope
/ Longitudinal Section Aspect
Condition: Stress Corrosion
×
Standard: AISI
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
54
VIEW
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M
- Austenitic Stainless Steel
P
- Stub End
Ap
- Chemical Industry
Cd
- Stress Corrosion
Cm
- Longitudinal Section Aspect
Df
- Multiple cracks