Identification drawing

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Identification drawingDf - Fracture
Schematic drawing presenting the longitudinal section of the shell plate (sample removed from the boiler), at the position of the fillet weld (sealing weld) with a tube,  where surface welding repairs created conditions for cracking the base material in a transgranular morphology. Several cracks were identify starting from the steam drum internal surface.
120
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Identification drawingDf - Cracks

More from these cases

ML00052 — Cold Cracks in API 5CT L80 Tube Welded to a Structural PartM - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Identification drawingDf - Welded Joint