Crevice Corrosion in a Subsea System — Aspect Before Analysis

The fracture surface is flat, shows the graphite nodules and cleavage of the ferritic microstructure, indicating that the material have exceeded the capacity to acomodate the stress.
945
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets

More from these cases

ML00040 — Brittle Fracture of a Valve StemM - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Detail of the cleavage micromechanism.
195
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets