Fractography by SEM

1 case · 3 images for “fracture”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Detail of the pin fracture surface, presenting both a flat aspect and a rough aspect in a shearing section of 2.5 mm width.
727
ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Fractography by SEMDf - Fracture

More from these cases

ML00046 — Brittle Fracture of SS Shear PinM - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Fracture appearance in a sheared region, presenting a ductile morphology for the fracture micromechanism.
109
ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Fractography by SEMDf - Ductile Fracture
ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Fractography by SEMDf - Intergranular Cracking