Fractography by SEM

3 cases · 8 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
Detail of the fracture surface, predominantly transgranular with secondary cracks of intergranular morphology.
831
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
The fracture surface, although presenting a large amount of corrosion products, shows also evidences of a brittle behavior with regions of cleavage micromechanism.
116
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

More from these cases

ML00134 — Brittle Fracture of a Superduplex Valve BodyM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Secondary Cracks
ML00078 — Hydrogen Cracking of IN 718 Subsea ConnectorM - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets