Fractography by SEM

1 case · 2 images for “hydrogen”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the fracture surface of the bolt, after cleaning with a  plastic brush.  Although there is a layer of oxides it is possible to see the intergranular morphology of the fracture, typical of a hydrogen embrittlement mechanism.
1154
ML00126 / Mar.2018
Hydrogen Fracture of Subsea Allen Bolts
M - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture

More from these cases

ML00126 — Hydrogen Fracture of Subsea Allen BoltsM - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Detailed aspect of the fracture surface of the bolt, evidencing the intergranular morphology of the fracture (although with an oxide scale), typical of a hydrogen embrittlement mechanism.
114
ML00126 / Mar.2018
Hydrogen Fracture of Subsea Allen Bolts
M - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture