Fracture surface after opening the shell cracking, presenting fatigue striation.  The fracture presents also foreign particles.
132
ML00050 / Nov.2017
Fatigue Failure of a 316SS Pressure Stabilizer
M - Austenitic Stainless SteelP - Fabrication WeldAp - Chemical IndustryCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation