Fractography by SEM

8 cases · 9 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking
ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking
ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking
ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Fractography by SEMDf - Intergranular Cracking
Fractographic aspect of the broken fastener, at the surface, showing na intergranular morphology typical of a hydrogen assisted mechanism of a high strenght steel under cathodic protection.
224
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Fractography by SEMDf - Intergranular Cracking
ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Fractography by SEMDf - Intergranular Cracking
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Intergranular Cracking

More from these cases

ML00009 — Hydrogen Cracking of a 5" Drill Pipe S135M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement