Fractography by SEM

5 cases · 15 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Brittle Fracture
ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface
Fractographic detail of the longitudinal Charpy V testpiece,  broken at -46°C and presenting energy of 64J (the average energy of three tespieces was 70J).  The Charpy V testpiece was removed from the center of the bar. The micromechanism is quasicleavage and the test in this direction presented energy values superior than the minimum requirement of 45J.
944
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Fractography by SEMDf - Fracture
ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Fractography by SEMDf - Intergranular Cracking

More from these cases

ML00148 — Brittle Fracture of a 420 SS Barrel NutM - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Fracture
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Fracture
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Intergranular Fracture
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Dimples
ML00131 — Brittle Failure of a Soft Roller BearingM - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the Internal Surface
ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the Internal Surface
ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface
ML00123 — Non Qualified Superduplex for SubseaM - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Fractography of the broken Charpy V testpiece,  longitudinal, broken at -46°C and presenting energy of 64J (the average of three values was 70J).  In this direction the material presented an energy value higher than the minimum requirement of 45J.
109
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece
Fractography of the Charpy V testpiece, transverse section, broken at -46°C and presenting energy of 20J (the average of three results was 33J).  The coarse structure and the alignement created a condition for low energy results in this specific direction, and the material did not present the minimum requirement of 45J.
103
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece
ML00071 — Reheating Cracking of a CrMo Vessel WeldM - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Fractography by SEMDf - Intergranular Cracking