Fractography by SEM
4 cases · 11 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets

ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece

ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
More from these cases

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Secondary Cracks

ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece

ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece

ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture