Fractography by SEM

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Ductile Fracture