Fractography by SEM
2 cases · 6 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Margin of the Weld Crack
More from these cases

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation