Field photo

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the waterwall during removal of the leaking tube. The leakage was detected, by visual inspection, from the outside of the boiler.
1675
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Field photoDf - General View

More from these cases

ML00163 — Corrosion Fatigue of a Boiler Waterwall TubeM - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Aspect of the sample removed from the waterwall, where the tube has leaked, presenting the crack in the membrane.
361
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Field photoDf - Through Wall Cracking