Aspect by NDT

2 cases · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Aspect by NDTDf - Crack
Aspect of the cracking after Dye Check Test (Liquid Penetrant) in the external side of the line that operates at 800°C, insulated, and presented the leakage associated to the longitudinal seam weld of the fitting. The circumferential butt weld of the fitting to a pipe did not fail. See the schematic drawing in the next figure
371
ML00061 / Apr.2017
Creep in a Seam Weld of a 304H SS Fitting
M - Austenitic Stainless SteelP - Fabrication WeldAp - Chemical IndustryCd - Creep
Cm - Aspect by NDTDf - Through Wall Cracking