Aspect Before Analysis

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the tube internal surface after removal from the boiler, presenting multiple longitudinal cracks.
295
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Aspect Before AnalysisDf - Internal Surface
Aspect of the superheater ND 1" tube that was in operation for about 35,000 hours and presented a thick deposit at the external surface.
211
ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Aspect Before AnalysisDf - General View

More from these cases

ML00163 — Corrosion Fatigue of a Boiler Waterwall TubeM - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Aspect of the external surface of the leaking tube, after removal of the membrane.
262
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Aspect Before AnalysisDf - External Surface