Aspect Before Analysis

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the superheater ND 1" tube that was in operation for about 35,000 hours and presented a thick deposit at the external surface.
211
ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Aspect Before AnalysisDf - General View