Oil and Gas
2 cases · 3 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by SEMDf - Martensite

ML00152 / Dec.2018
Low Alloy Steel Pump Shaft
M - High Strength Low AlloyP - ShaftAp - Oil and GasCd - Removed From Service
Cm - Nital Etched Micrography by SEMDf - Pearlite
More from these cases

ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by SEMDf - Martensite