Oil and Gas
3 cases · 4 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture

ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Fracture
More from these cases