Offshore
4 cases · 9 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00113 / Jan.2018
Autogenous Weld of a Carbon Steel Wire
M - Medium Carbon SteelP - WireAp - OffshoreCd - Welding
Cm - Nital Etched Micrography by OMDf - Heat Affected Zone

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Heat Affected Zone

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Heat Affected Zone

ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Heat Affected Zone
More from these cases

ML00113 / Jan.2018
Autogenous Weld of a Carbon Steel Wire
M - Medium Carbon SteelP - WireAp - OffshoreCd - Welding
Cm - Nital Etched Micrography by OMDf - Heat Affected Zone

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Heat Affected Zone

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Heat Affected Zone

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Surface Aspect by SEMDf - Heat Affected Zone

ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Heat Affected Zone