Offshore
2 cases · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Damage ×Capture method: Aspect Before Analysis ×Detail focus: External Surface ×clear all

ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Aspect Before AnalysisDf - External Surface

ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Aspect Before AnalysisDf - External Surface